Connect symptoms to tool condition
Flash, parting step, drag marks and dimensional drift can point to wear, damage or alignment issues, but each also has other possible causes. Compare the affected cavity and feature with process records and the tool inspection. Reworking steel before identifying the cause can remove useful evidence.
Make repair a controlled change
Record the location, reason and scope of maintenance. Identify replaced inserts and any changed geometry. After work, verify the affected dimensions, appearance, release and downstream machining. Retain the repair record with the tool history so the next order does not inherit an undocumented process change.
Review checklist
| Review item | Define before release | Evidence to retain |
|---|---|---|
| Trend | Cavity, feature and sample sequence | Inspection history |
| Repair | Steel change or insert replacement | Approved maintenance record |
| Return to service | Affected dimensions and function | Post-repair acceptance |
Worked review example
Growing flash at one slide shutoff should be compared with slide condition and alignment. Tightening a general appearance limit without repairing the cause will not stabilize production.
Apply the review to your drawing
Identify the affected features on the current drawing and attach the material, finish and operating requirements that control them. Agree the proposed route and acceptance evidence before releasing a change. Send the controlled files for a project review.