Look at the temperature pattern
A die has local hot and cold regions, not one uniform operating temperature. Thick junctions, thin extremities, cooling circuits and spray practice influence the pattern. Correlate temperature observations with sample location and process stage. A single reading taken after a long stop may not represent stable production.
Control startup and interruptions
Define how the die reaches its intended operating condition and what happens after a stop. Record relevant process settings and identified samples during trials. Changes to cooling, lubrication or cycle sequence should be evaluated together so a surface improvement does not create a dimensional or filling problem elsewhere.
Review checklist
| Review item | Define before release | Evidence to retain |
|---|---|---|
| Startup | Warmup state and first acceptable parts | Startup acceptance record |
| Local defect | Location and thermal observations | Trial comparison |
| Process change | Cooling, spray and cycle settings | Approved operating window |
Worked review example
A cold-shut pattern that appears only after a pause needs a restart investigation. Changing the steady-state cycle without separating the restart samples can obscure the cause.
Apply the review to your drawing
Identify the affected features on the current drawing and attach the material, finish and operating requirements that control them. Agree the proposed route and acceptance evidence before releasing a change. Send the controlled files for a project review.